46 C.F.R. §§ 56.60-5

Current through September 30, 2024
Section 56.60-5 - Steel (High temperature applications)
(a) (Reproduces 124.2.A.) Upon prolonged exposure to temperatures above 800 °F (427 °C), the carbide phase of plain carbon steel, plain nickel-alloy steel, carbon-manganese-alloy steel, manganese-vanadium-alloy steel, and carbon-silicon steel may convert to graphite.
(b) (Reproduces 124.2.B.) Upon prolonged exposure to temperatures above 875 °F (468 °C), the carbide phase of alloy steels, such as carbon-molybdenum, manganese-molybdenum-vanadium, manganese-chromium-vanadium, and chromium-vanadium, may convert to graphite.
(c) The design temperature of a piping system employing one or more of the materials listed in paragraphs (a) and (b) of this section must not exceed the lowest graphitization temperature specified for materials used.

46 C.F.R. §§56.60-5

CGFR 68-82, 33 FR 18843, Dec. 18, 1968, as amended by CGFR 69-127, 35 FR 9978, June 17, 1970; CGD 72-104R, 37 FR 14233, July 18, 1972; CGD 73-248, 39 FR 30839, Aug. 26, 1974; CGD 73-254, 40 FR 40165, Sept. 2, 1975; USCG-2003-16630, 73 FR 65183, Oct. 31, 2008
89 FR 50153, 9/10/2024